标题:Optimisation of ITER Nb3Sn CICCs for coupling loss, transverse electromagnetic load and axial thermal contraction

作者:A. Nijhuis, E. P. A. van Lanen, G. Rolando
查看论文《Optimisation of ITER Nb3Sn CICCs for coupling loss, transverse electromagnetic load and axial thermal contraction》的 PDF
查看原文 PDF 中文 PDF (下批处理) EasyResearch 阅读
摘要:The ITER cable-in-conduit conductors (CICCs) are built up from sub-cable bundles, wound in different stages, which are twisted to counter coupling loss caused by time-changing external magnet fields. The selection of the twist pitch lengths has major implications for the performance of the cable in the case of strain sensitive superconductors, i.e. Nb3Sn, as the electromagnetic and thermal contraction loads are large but also for the heat load from the AC coupling loss. Reduction of the transverse load and warm-up cool-down degradation can be reached by applying longer twist pitches in a particular sequence for the sub-stages, offering a large cable transverse stiffness, adequate axial flexibility and maximum allowed lateral strand support. Analysis of short sample (TF conductor) data reveals that increasing the twist pitch can lead to a gain of the effective axial compressive strain of more than 0.3 % with practically no degradation from bending. For reduction of the coupling loss, specific choices of the cabling twist sequence are needed with the aim to minimize the area of linked strands and bundles that are coupled and form loops with the applied changing magnetic field, instead of simply avoiding longer pitches. In addition we recommend increasing the wrap coverage of the CS conductor from 50 % to at least 70 %. The models predict significant improvement against strain sensitivity and substantial decrease of the AC coupling loss in Nb3Sn CICCs, but also for NbTi CICCs minimization of the coupling loss can be achieved. Although the success of long pitches to transverse load degradation was already demonstrated, the prediction of the combination with low coupling loss needs to be validated by a short sample test.
评论: to be published in Supercond Sci Technol
主题: 加速器物理 (physics.acc-ph)
引用方式: arXiv:1110.3205 [physics.acc-ph]
  (或者 arXiv:1110.3205v1 [physics.acc-ph] 对于此版本)
  https://doi.org/10.48550/arXiv.1110.3205
相关 DOI: https://doi.org/10.1088/0953-2048/25/1/015007

提交历史

来自:Arend Nijhuis
[v1] 2011年10月13日 星期四 12:10:02 UTC
全文链接:

访问论文:

  • 查看原文 PDF
  • 中文 PDF (下批处理)
  • EasyResearch 阅读
  • TeX 源文件
  • arXiv 原文页面
查看许可

当前浏览上下文:

physics.acc-ph
< 上一篇   |   下一篇 >
最新 | 近期 | 2011-10
切换浏览方式为:
physics

参考文献与引用

  • Google Scholar
  • Semantic Scholar

BibTeX 格式的引用

EasyXiv 是独立运营的中文预印本站点,与 arXiv 及康奈尔大学无隶属关系。 论文元数据与原文来自 arXiv.org,感谢 arXiv 提供开放获取服务。
关于 · 帮助 · 投稿指南 · 版权 · arXiv 原站