物理学 > 应用物理
[提交于 2017年12月11日]
标题:Selective etching of PDMS: etching as positive resist
查看原文 PDF 中文 PDF (下批处理) EasyResearch 阅读摘要:Although, poly(dimethylsiloxane) (PDMS) is a widely used material in numerous applications, such as micro- or nanofabrication, the method of its selective etching has not been known up to now. In this work authors present two methods of etching the pure, additive-free and cured PDMS as a positive resist material. To achieve the chemical modification of the polymer necessary for selective etching, energetic ions were used. We created 7 um and 45 um thick PDMS layers and patterned them by a focused proton microbeam with various, relatively large fluences. In this paper authors demonstrate that 30 wt% Potassium Hydroxide (KOH) or 30 wt% sodium hydroxide (NaOH) at 70 oC temperature etch proton irradiated PDMS selectively, and remove the chemically sufficiently modified areas. In case of KOH development, the maximum etching rate was approximately 3.5 um/minute and it occurs at about 7.5*10^15 ion*cm-2. In case of NaOH etching the maximum etching rate is slightly lower, 1.75 um/minute and can be found at the slightly higher fluence of 8.75*10^15 ion*cm-2. These results are of high importance since up to this time it has not been known how to develop the additive-free, cross-linked poly(dimethylsiloxane) in lithography as a positive tone resist material.
提交历史
来自:Szabolcs Szilasi Dr[v1] 2017年12月11日 星期一 00:00:00 UTC