标题:Asynchronous Lock In Thermography of 3D Printed PLA and ABS samples

作者:K. H. H. Goh, Q. F. Lim, P. K. Pallathadka
查看论文《Asynchronous Lock In Thermography of 3D Printed PLA and ABS samples》的 PDF
查看原文 PDF 中文 PDF (下批处理) EasyResearch 阅读
摘要:Lock-In thermography is a useful Non Destructive Technique (NDT) for enhanced detection of defects in components, as it amplifies the phase contrast where defects exist. This amplification was found to be around 2-3 times compared to constant heating. The current used a Fuse Deposition Modelling (FDM) 3D printer to print samples with known defects, in order to characterise the relative effects of different variables on the Lock-In phase data. Samples were printed using ABS (Acrylonitrile Butadiene Styrene) and PLA (Polylactic Acid) for comparisons, and variables such as print direction, cameras, heating power, Lock-In frequency, as well as thickness, width and depth of defects were explored. It was found that different materials resulted in different baselines, but had similar phase contrast. A novel asynchronous technique was derived to enable Lock-In measurements with 5 different infrared cameras, and similar results were found. Even cheap cameras like the Seek Thermal CompactXR were proven capable of detecting the same defects as other cameras such as the FLIR SC7500. Heating power did not affect phase contrast, except for shallower defects up to 1.0 mm deep, where higher power resulted in better contrast. As expected, deeper defects could only be detected using lower Lock-In frequencies, and there was better phase contrast with wider, thicker and shallower defects. It was shown that defects 4 mm in width could be detected automatically up to a depth of around 1.5 mm, based on the phase signal trends. Sub-sampling of frame data showed that at least 10 frames were required per Lock-In period for minimal deviations in Lock-In phase contrast. Also, it was shown that phase contrast was similar for shallower defects up to 1.5 mm deep, with data from 1 Lock-In period, as long as the first frame was synchronised with the heating cycle.
主题: 应用物理 (physics.app-ph); 经典物理 (physics.class-ph)
引用方式: arXiv:1805.01343 [physics.app-ph]
  (或者 arXiv:1805.01343v1 [physics.app-ph] 对于此版本)
  https://doi.org/10.48550/arXiv.1805.01343

提交历史

来自:Kok Hin Henry Goh
[v1] 2018年5月4日 星期五 00:00:00 UTC
全文链接:

访问论文:

  • 查看原文 PDF
  • 中文 PDF (下批处理)
  • EasyResearch 阅读
  • TeX 源文件
  • arXiv 原文页面
查看许可

当前浏览上下文:

physics.app-ph
< 上一篇   |   下一篇 >
最新 | 近期 | 2018-05
切换浏览方式为:
physics
physics.class-ph

参考文献与引用

  • Google Scholar
  • Semantic Scholar

BibTeX 格式的引用

EasyXiv 是独立运营的中文预印本站点,与 arXiv 及康奈尔大学无隶属关系。 论文元数据与原文来自 arXiv.org,感谢 arXiv 提供开放获取服务。
关于 · 帮助 · 投稿指南 · 版权 · arXiv 原站