标题:Structural, dielectric and ferroelectric studies of thermally stable and efficient energy storage ceramic material: (Na0.5-xKxBi0.5-xLax)TiO3

作者:Anita Verma, Arun Kumar Yadav, Nasima Khatun, Sunil Kumar, Ravindra Jangir, Velaga Srihari, V. Raghavendra Reddy, Shun Wei Liu, Sajal Biring, Somaditya Sen
查看论文《Structural, dielectric and ferroelectric studies of thermally stable and efficient energy storage ceramic material: (Na0.5-xKxBi0.5-xLax)TiO3》的 PDF
查看原文 PDF 中文 PDF (下批处理) EasyResearch 阅读
摘要:The structural, dielectric and ferroelectric properties of lead-free (Na0.5-xKxBi0.5-xLax)TiO3 powders synthesized by sol-gel self-combustion method were investigated. Rietveld refinement of Synchrotron x-ray diffraction data confirms pure single phase rhombohedral crystal structure with R3c space group for all the compositions and anti-phase octahedral tilting angle decreased with increase in composition x. Homogeneity and elemental proportions were confirmed by Energy dispersive x-ray spectrometry. The temperature-dependent dielectric study has shown two diffuse type of dielectric anomaly for all the samples, due to A-site disorder in the lattice, which has been assigned to two-has transitions: ferroelectric to anti-ferroelectric and anti-ferroelectric to the paraelectric phase transition. The transition temperature of these phase transitions is found to decrease as a function of composition. Thermal stability range of dielectric constant increases from ~100C to 220C as a function of composition. Stable dielectric constant first increases, from 1557 10 % for parent compound, with the composition, highest for 6 % composition with emid ~ 2508 10 % for the temperature range ~180 C to 340C and after that decreases to 1608 10 % for 12 % but remain higher than the parent compound Na0.5Bi0.5TiO3. Ferroelectric measurements have shown monotonously decreasing coercive field as a function of the composition due to a decrease in grain size, confirmed by microstructural studies using Field Emission Scanning Electron Microscope. Exponential increases in the energy storage efficiency from ~ 17 % to 87 % as a function of composition have also observed. These types of materials, with stable high dielectric constant and low tan delta, have a vast scope in the field of the thermally stable dielectric constant materials and energy storage applications.
评论: 18 Pages, 8 figures , 4 tables
主题: 材料科学 (cond-mat.mtrl-sci)
引用方式: arXiv:1806.00587 [cond-mat.mtrl-sci]
  (或者 arXiv:1806.00587v1 [cond-mat.mtrl-sci] 对于此版本)
  https://doi.org/10.48550/arXiv.1806.00587

提交历史

来自:Somaditya Sen
[v1] 2018年6月5日 星期二 00:00:00 UTC
全文链接:

访问论文:

  • 查看原文 PDF
  • 中文 PDF (下批处理)
  • EasyResearch 阅读
  • TeX 源文件
  • arXiv 原文页面
查看许可

当前浏览上下文:

cond-mat.mtrl-sci
< 上一篇   |   下一篇 >
最新 | 近期 | 2018-06
切换浏览方式为:
cond-mat

参考文献与引用

  • Google Scholar
  • Semantic Scholar

BibTeX 格式的引用

EasyXiv 是独立运营的中文预印本站点,与 arXiv 及康奈尔大学无隶属关系。 论文元数据与原文来自 arXiv.org,感谢 arXiv 提供开放获取服务。
关于 · 帮助 · 投稿指南 · 版权 · arXiv 原站