标题:Sn-Doping in LPCVD-Grown (010) $\beta$-Ga$_2$O$_3$ Films

作者:Saleh Ahmed Khan, Ahmed Ibreljic, Sourav Sarker, Anhar Bhuiyan
查看论文《Sn-Doping in LPCVD-Grown (010) $\beta$-Ga$_2$O$_3$ Films》的 PDF
查看原文 PDF 中文 PDF (下批处理) EasyResearch 阅读
摘要:In this work, Sn-doped (010) $\beta$-Ga$_2$O$_3$ homoepitaxial films were grown by low-pressure chemical vapor deposition (LPCVD), and the influence of Sn incorporation on their structural, morphological, and electrical properties was systematically investigated. Controlled room-temperature carrier concentrations ranging from $1.17 \times 10^{17}$ to $3.06 \times 10^{18}$ cm$^{-3}$ were achieved, with corresponding Hall mobilities decreasing from 113 to 63 cm$^2$ V$^{-1}$ s$^{-1}$. The films exhibited the monoclinic $\beta$-Ga$_2$O$_3$ phase, near-stoichiometric composition, and well-defined step-flow morphology, with a minimum rocking-curve FWHM of 68.4 arcsec and an RMS roughness of 2.63 nm. Film thicknesses ranging from 1.66 to 11.3 $\mu$m were obtained at growth rates of 6.4 to 16.6 $\mu$m h$^{-1}$, demonstrating the ability of LPCVD to produce thick epitaxial layers. The sample with a room-temperature carrier concentration of $1.17 \times 10^{17}$ cm$^{-3}$ exhibited room-temperature and low-temperature Hall mobilities of 113 cm$^2$ V$^{-1}$ s$^{-1}$ and 380 cm$^2$ V$^{-1}$ s$^{-1}$ at 84 K, respectively. Both represent the highest reported values for LPCVD-grown Sn-doped $\beta$-Ga$_2$O$_3$. Transport modeling of the same sample yielded a shallow donor activation energy of 32.7 meV, a deeper donor level at 95 meV, and a low compensating acceptor concentration of $2.0 \times 10^{16}$ cm$^{-3}$, indicating efficient donor activation and a low degree of compensation. These results demonstrate that LPCVD enables controlled Sn doping while maintaining excellent structural and electrical quality, providing a viable route for realizing thick $\beta$-Ga$_2$O$_3$ epitaxial drift layers.
主题: 材料科学 (cond-mat.mtrl-sci); 应用物理 (physics.app-ph)
引用方式: arXiv:2608.07823 [cond-mat.mtrl-sci]
  (或者 arXiv:2608.07823v1 [cond-mat.mtrl-sci] 对于此版本)
  https://doi.org/10.48550/arXiv.2608.07823

提交历史

来自:Anhar Bhuiyan
[v1] 2026年8月7日 星期五 23:52:29 UTC
全文链接:

访问论文:

  • 查看原文 PDF
  • 中文 PDF (下批处理)
  • EasyResearch 阅读
  • TeX 源文件
  • arXiv 原文页面
查看许可

当前浏览上下文:

cond-mat.mtrl-sci
< 上一篇   |   下一篇 >
最新 | 近期 | 2026-08
切换浏览方式为:
cond-mat
physics.app-ph

参考文献与引用

  • Google Scholar
  • Semantic Scholar

BibTeX 格式的引用

EasyXiv 是独立运营的中文预印本站点,与 arXiv 及康奈尔大学无隶属关系。 论文元数据与原文来自 arXiv.org,感谢 arXiv 提供开放获取服务。
关于 · 帮助 · 投稿指南 · 版权 · arXiv 原站